search  current discussion  categories  techniques - spraying 

paasche l sprayer tip size (answer)

updated thu 2 aug 01

 

Fabienne Micheline Cassman on wed 1 aug 01


Greetings,

I spoke to the people at Paasche; it turns out they are almost in my
backyard :) The tip to use is #4, i.e. the largest one because glaze are
considered the heaviest of all liquids this line can handle. The part
number is: L#4 and the cup that goes with it is one quart, L-SC#4QT. The
hose to use is HL-3/16 various lengths, some with coupling and others
without depending on your needs.

Their site is http://www.paascheairbrush.com/

Cheers,

Fabienne


--
Milky Way Ceramics http://www.milkywayceramics.com/

Yes, I have learned from my mistakes...
I can reproduce them exactly.