search  current discussion  categories  kilns & firing - raku 

texture raku which might solve your problem!

updated tue 31 jul 01

 

Chris Stanley on mon 30 jul 01


Here is one of my stock texture raku recipes:
Texture Glaze
Gerstley borate 4
Bone Ash 3
Copper Carbonate 1
Even though this one has Gerstley Borate in it, the Bone Ash keeps
it balled up and crawly!
Just a thick coat with a big house paint brush and there is the look I think
you are after!