Tom Herndon on sat 4 aug 01
Howdy,
Looking for an additive for my current clay body (cone 8, ox.) that will make
it an orange-ish, terra cotta color. Is there such an animal, or does
everything burn out at that temp?
Thank you in advance for any & all info on this subject,
Tom
Karen Sullivan on sat 4 aug 01
Tom..
would Iron Oxide work?
on 8/4/01 10:00 AM, Tom Herndon at TomHerndon01@AOL.COM wrote:
> Howdy,
>
> Looking for an additive for my current clay body (cone 8, ox.) that will make
> it an orange-ish, terra cotta color. Is there such an animal, or does
> everything burn out at that temp?
>
> Thank you in advance for any & all info on this subject,
> Tom
>
> ______________________________________________________________________________
> Send postings to clayart@lsv.ceramics.org
>
> You may look at the archives for the list or change your subscription
> settings from http://www.ceramics.org/clayart/
>
> Moderator of the list is Mel Jacobson who may be reached at
> melpots@pclink.com.
| |
|