Alisa og Claus Clausen on thu 9 aug 01


Sorry, no only one time Flint 5. =20
Good people are sharp on the list.

> Alisha -
> In your second recipe for Teadust....there are two flints at 5 =
each....is
> this correct
>=20
> > Fired to 1220c oxidation.
> >
>=20
> >
> > Tea Dust
> > 50 Potash
> > 15 China clay
> > 5 Flint
> > 5 Flint
> > 15 Whiting
> >
> > ADD
> > 5 RIO
> > 5 Manganese diox.
> > 5 cobalt ox.
> >
> > Best regards,
> > Alisa in Denmark
> >
> >
> =
_________________________________________________________________________=

> _____
> > Send postings to clayart@lsv.ceramics.org
> >
> > You may look at the archives for the list or change your
> > subscription
> > settings from http://www.ceramics.org/clayart/
> >
> > Moderator of the list is Mel Jacobson who may be reached at
> > melpots@pclink.com.
> >
> ________________________________________________________________
> GET INTERNET ACCESS FROM JUNO!
> Juno offers FREE or PREMIUM Internet access for less!
> Join Juno today! For your FREE software, visit:
> http://dl.www.juno.com/get/tagj.
>=20
> =
_________________________________________________________________________=
_____
> Send postings to clayart@lsv.ceramics.org
>=20
> You may look at the archives for the list or change your subscription
> settings from http://www.ceramics.org/clayart/
>=20
> Moderator of the list is Mel Jacobson who may be reached at =
melpots@pclink.com.
>=20