search  current discussion  categories  glazes - specific colors 

wonder white

updated mon 13 aug 01

 

ASHPOTS@AOL.COM on sun 12 aug 01


I have been using wonder white from Highwater for 2 tons so far. I had tried
a bunch of Highwater clays. My ash glazes look great on it. I find it easy to
work with also. I have no problems with attaching handles. I make pulled
handles and also a coil handle on my work.
My last batch was stiff so i run it thru my Venco adding water. I have been
making lots of 16 to 20 inch platters so i needed it more soft.
Wonder White works for me

Capt Mark
Lookout Mountain Pottery
Rising Fawn Ga