> Allo Lorraine,
>
> Bleu Dean:
>
> Custer spar 65
> Barium carbonate 35
>
> Bentonite 3
> Copper oxide 4.35
>
>
> Later,
>
>
> Edouard Bastarache
> Irreductible Quebecois
> Sorel-Tracy
> Quebec
> edouardb@sorel-tracy.qc.ca
> http://sorel-tracy.qc.ca/~edouardb/
> http://www.absolutearts.com/portfolios/e/edouardb/
>
>
____________________________________________________________________________
__
> Send postings to clayart@lsv.ceramics.org
>
> You may look at the archives for the list or change your subscription
> settings from http://www.ceramics.org/clayart/
>
> Moderator of the list is Mel Jacobson who may be reached at
melpots@pclink.com.

Lorraine Pierce on wed 29 aug 01


Hi Eduardo...cannot find the copy I had of your ^10 red. Bleu Dean glaze.
Can you tell me where to get a copy of the recipe? Thanks, Lori Pierce in
New Port Richey, Fl.

Edouard Bastarache on wed 29 aug 01


Allo Lorraine,

Bleu Dean:

Custer spar 65
Barium carbonate 35

Bentonite 3
Copper oxide 4.35


Later,


Edouard Bastarache
Irreductible Quebecois
Sorel-Tracy
Quebec
edouardb@sorel-tracy.qc.ca
http://sorel-tracy.qc.ca/~edouardb/
http://www.absolutearts.com/portfolios/e/edouardb/

Ron Roy on thu 30 aug 01


Good grief - try some lemon juice on this and tell us how long it takes to
lose the colour.

RR


>Bleu Dean:
>
>Custer spar 65
>Barium carbonate 35
>
>Bentonite 3
>Copper oxide 4.35

Ron Roy
RR# 4
15084 Little Lake Rd..
Brighton,
Ontario, Canada
KOK 1H0
Residence 613-475-9544
Studio 613-475-3715
Fax 613-475-3513

Edouard Bastarache on thu 30 aug 01


Who says I use it on utilitarian wares?


Later,


Edouard Bastarache
Irreductible Quebecois
Sorel-Tracy
Quebec
edouardb@sorel-tracy.qc.ca
http://sorel-tracy.qc.ca/~edouardb/
http://www.absolutearts.com/portfolios/e/edouardb/

----- Original Message -----
From: Ron Roy
To:
Sent: Thursday, August 30, 2001 6:32 PM
Subject: Re: Blue Dean


> Good grief - try some lemon juice on this and tell us how long it takes to
> lose the colour.
>
> RR
>
>
> >Bleu Dean:
> >
> >Custer spar 65
> >Barium carbonate 35
> >
> >Bentonite 3
> >Copper oxide 4.35
>
> Ron Roy
> RR# 4
> 15084 Little Lake Rd..
> Brighton,
> Ontario, Canada
> KOK 1H0
> Residence 613-475-9544
> Studio 613-475-3715
> Fax 613-475-3513
>
>
____________________________________________________________________________
__
> Send postings to clayart@lsv.ceramics.org
>
> You may look at the archives for the list or change your subscription
> settings from http://www.ceramics.org/clayart/
>
> Moderator of the list is Mel Jacobson who may be reached at
melpots@pclink.com.