Merrie Boerner on fri 31 aug 01
Tony wrote..."If I had a dog of a kiln I'd contact Lowell and get the
vacuum/sawdust
happening. Only thing is I hate the sound of a vacuum more than any other
sound."
When you play good music and enjoy sunbathing in the lounge chair during the
sawdust firing...you don't notice the sound of the blower. It's hot, it
works.
Merrie
we play pink Floyd really loud when we vacuum.
Steve Dalton on fri 31 aug 01
Tony,
Where would one find this book? Would Steve with the Potter's Shop have it?
Steve Dalton
Clear Creek Pottery
Snohomish, WA
sdpotter@gte.net
----------
> From: clennell
> To: CLAYART@LSV.CERAMICS.ORG
> Subject: Little trains
> Date: Thu, 30 Aug 2001 09:35:50 +0800
>
>Wood-fired Ceramics by Coll Minogue and Robert
>Sanderson.
clennell on fri 31 aug 01
Sour Cherry Pottery
> Where would one find this book? Would Steve with the Potter's Shop have it?
> Steve Dalton
> Clear Creek Pottery
> Snohomish, WA
> sdpotter@gte.net
>
> ----------
>Dear Steve: Does a bear poop in the woods??? you bet he'll have it or get it
pronto! Just had three people here today thinking about a wood kiln. took a
look at the book and they off to build the long train shown in the book .
Best of luck.
tony
P>S> If i had a dog of a kiln I'd contact Lowell and get the vacuum/sawdust
happening. Only thing is I hate the sound of a vacuum more than any other
sound.
becky schroeder on fri 31 aug 01
steve,
amazon has it. i tried steve at Potter's shop but they are out of town for
awhile. drat!
becky schroeder
>
>Tony,
>Where would one find this book? Would Steve with the Potter's Shop have
>it?
>----------
> >
> >Wood-fired Ceramics by Coll Minogue and Robert
> >Sanderson.
>
>______________________________________________________________________________
>Send postings to clayart@lsv.ceramics.org
>
>You may look at the archives for the list or change your subscription
>settings from http://www.ceramics.org/clayart/
>
>Moderator of the list is Mel Jacobson who may be reached at
>melpots@pclink.com.
_________________________________________________________________
Get your FREE download of MSN Explorer at http://explorer.msn.com/intl.asp
| |
|