I'm currently off the clayart list, but came across your inquiry =
regarding BNZ insulating bricks. I work for an Industrial kiln builder =
and have had excellent luck with BNZ brick for the last 5 years. BNZ is =
the only company I am aware of whose main product is insulating brick. =
All of the others - Thermal, Newcastle, AP Green make mostly other =
products, and by the way, can sell you IFB also. Our brick layers like =
the feel of the BNZ brick, they cut easily and dont crumble too much. We =
haven't had any problems in any of the kilns and furnaces (up to 2800 =
deg) we have lined with BNZ. Feel free to email back with any questions =
or comments.=20