Marianne Lombardo on wed 5 sep 01
Thanks! I will get it.
Thanks to everyone for the help with making plaster bats. I will try making
one next week, and see how it works.
Marianne
----- Original Message -----
From: "C TRIPP"
To:
Sent: Tuesday, September 04, 2001 10:28 AM
Subject: Re: Making Plaster Bats
> Hi Marianne,
> Please get a copy of Pottery Making Illustrated Spring 2001 in which you
> will find an article "Making Plaster Bats". I might add that if you are
not
> already subscribing to this magazine, then you should be. And all the back
> issues are worth getting too. It is full of useful information.
> (www.potterymaking.org)
> It is well worth the money. No, I don't work for them.
> Good luck,
> Carol
| |
|