search  current discussion  categories  glazes - misc 

glaze test result

updated thu 6 sep 01

 

Marianne Lombardo on wed 5 sep 01


Here is a lovely, interesting layering effect that I just tried. Falls =
Creek Fake Shino, with a 1/2" band of Oxblood Red at the top of the pot, =
on the outside. On Tucker's red ^6 stoneware the shino portion is a =
nice creamy with rust breaking through, and the Oxblood runs (a lot) =
over it, becoming a pretty non-metallic copper colour, and at the bottom =
of the run it feathers out. Very pretty.

Before I get tons of emails asking for the recipes, here is the web site =
link to Stephen Pilachowski's web site where I saw his beautiful =
pictures, and obtained the recipe. Thank's, Stephen.

http://members.bellatlantic.net/~spilacho/glazes.htm

Marianne Lombardo
Omemee, Ontario, Canada
email: mlombardo@nexicom.net