teri frame on sat 6 oct 01


Chris,
I havn't seen it go yellow yet, but it sounds like the
one you're looking for.

Copper Blue Matt Glaze II ^9

Barium carb 30
Kingman spar 60
Neph sye 5
EPK 5

Copper carb 6

__________________________________________________
Do You Yahoo!?
NEW from Yahoo! GeoCities - quick and easy web site hosting, just $8.95/month.
http://geocities.yahoo.com/ps/info1

chris clarke on sun 7 oct 01


You are exactly right, that's it! And it's a Richard Fairbanks glaze. It
goes yellow where it's thinnest. I love this glaze on non food surfaces.
Thanks. chris


temecula, california
chris@ccpots.com
www.ccpots.com




----- Original Message -----
From: teri frame
To:
Sent: Saturday, October 06, 2001 12:07 AM
Subject: Found: Lost Glaze Recipe


> Chris,
> I havn't seen it go yellow yet, but it sounds like the
> one you're looking for.
>
> Copper Blue Matt Glaze II ^9
>
> Barium carb 30
> Kingman spar 60
> Neph sye 5
> EPK 5
>
> Copper carb 6
>
> __________________________________________________
> Do You Yahoo!?
> NEW from Yahoo! GeoCities - quick and easy web site hosting, just
$8.95/month.
> http://geocities.yahoo.com/ps/info1
>
>
____________________________________________________________________________
__
> Send postings to clayart@lsv.ceramics.org
>
> You may look at the archives for the list or change your subscription
> settings from http://www.ceramics.org/clayart/
>
> Moderator of the list is Mel Jacobson who may be reached at
melpots@pclink.com.