iandol on mon 8 oct 01
Dear Ralph Loewenthal,
You say <to you and your neighbours.>>
I agree. At close quarters such kiln effluents can have a very bad =
effect on your respiratory system.
But the big problem with both Sodium chloride and the Sodium carbonate =
vapour glazing is that the chemistry we read about or are taught about =
has never been validated by laboratory investigations. Yet many people =
accept it as a true fact. Writing published to support the old theories =
does not have necessary exclusive controls applied by scientific method.
As I have written before, until this work has been done we will always =
be prevented from using these valid ceramic methods by ignorant officers =
of whichever State we live in, unless categorical research is completed.
Best regards,
Ivor Lewis. Redhill, South Australia
| |
|