search  current discussion  categories  glazes - other named glazes 

gold lustre (on bisque)

updated tue 16 oct 01

 

Valice Raffi on mon 15 oct 01


Pam and all...

lusters WILL take on bisque, but of course they won't look lustery. I've
used them that way on sculptures & they have given the piece a subtle
metallic look similar to the look of matt metallic raku'd pieces.

Valice
in Sacramento

>
> To glaze it on, you need to apply on an already glazed surface =F1 it won=
=EDt
>take on bisque. (snip)
>Pam in Seattle