Ababi on sat 20 oct 01
I added part of my raku soil clayboy with lichen glaze to my raku page
and some slides to my stoneware page
Ababi Sharon
Kibbutz Shoval- Israel
Glaze addict
sharon@shoval.org.il
http://members4.clubphoto.com/ababi306910/
I would like to correct myself. Yesterday I made a raku firing for 4
test tiles as was not sure about some results. I found out that the
reason that some of the 80/20 glaze on porcelain was gray was because
of the color of the raku porcelain. I tested VC raku with some options,
I must see carefully which kaolin ( I guess the D'arvor) makes the body
gray.
Ababi
| |
|