Diana Pancioli on mon 29 oct 01


Dear Clayarters

I have misplaced my recipe for cone 10 crackle slip. I used is briefly in
the 80's and now my students want to try it. Does anyone have it handy?
I tried the archive to no avail (my own incompetence with the archive).

Thanks.

Diana

Ababi on mon 29 oct 01


This one from Penland glaze book
Borax 500
Zircopax 500
Custer feldspar 2000
Om-4 1500
Calcined Kaolin 1500
EPK 1500
flint 2000
Works fine in ^6
Ababi

---------- Original Message ----------

>Dear Clayarters

>I have misplaced my recipe for cone 10 crackle slip. I used is briefly
>in
>the 80's and now my students want to try it. Does anyone have it handy?
>I tried the archive to no avail (my own incompetence with the archive).

>Thanks.

>Diana

>________________________________________________________________________
>______
>Send postings to clayart@lsv.ceramics.org

>You may look at the archives for the list or change your subscription
>settings from http://www.ceramics.org/clayart/

>Moderator of the list is Mel Jacobson who may be reached at
>melpots@pclink.com.

Ababi on tue 30 oct 01


To be applied on bisque
---------- Original Message ----------

>This one from Penland glaze book
>Borax 500
>Zircopax 500
>Custer feldspar 2000
>Om-4 1500
>Calcined Kaolin 1500
>EPK 1500
>flint 2000
>Works fine in ^6
>Ababi

>---------- Original Message ----------

>>Dear Clayarters

>>I have misplaced my recipe for cone 10 crackle slip. I used is briefly
>>in
>>the 80's and now my students want to try it. Does anyone have it
>handy?
>>I tried the archive to no avail (my own incompetence with the archive).

>>Thanks.

>>Diana

>>_______________________________________________________________________
>_
>>______
>>Send postings to clayart@lsv.ceramics.org

>>You may look at the archives for the list or change your subscription
>>settings from http://www.ceramics.org/clayart/

>>Moderator of the list is Mel Jacobson who may be reached at
>>melpots@pclink.com.

>________________________________________________________________________
>______
>Send postings to clayart@lsv.ceramics.org

>You may look at the archives for the list or change your subscription
>settings from http://www.ceramics.org/clayart/

>Moderator of the list is Mel Jacobson who may be reached at
>melpots@pclink.com.