search  current discussion  categories  materials - frits 

ferro frit 4124

updated thu 1 nov 01

 

Graeme Anderson on wed 31 oct 01


According to my Ferro data sheets, (about1991) KGF 4124 is similar to KGF
4108, but not as reactive to glaze stains. Produces a milky gloss when
used alone - ie. 1020 to 1120 C.

Glaze frits are classified as follows.
Series KGF 4000 Clear Lead bearing.
Series KGF 4100 Clear Leadless.
Series KGF 9000 Semi opaque
Series KGF 9100 Opaque.

Cheers. Graeme.