search  current discussion  categories  materials - frits 

frit 3191

updated sun 11 nov 01

 

Tjo62@AOL.COM on fri 9 nov 01


Help....I want to mix a glaze that calls for frit 3191 and I don't have any.
We no longer have a distributer here in Louisville and I was wondering if
there was a comparable substitute. Thanks! Tonya

Ababi on fri 9 nov 01


This is from The Magic Of Fire by tony Hansen

FRIT 3191
Description: LEADLESS
Date: 09/05/97
Supplier: FERRO
Raw Weight: 248.85
Family: 5-Frit
ANALYSIS & UNITY FORMULA
CaO....... 11.27% [ 0.50]
Na2O...... 12.46% [ 0.50]
B2O3...... 27.97% 1.00
SiO2...... 48.30% 2.00
FRIT 3191 Notes
A source of alkali borate intended for use in abrasives
industry.
Sub: Fusion F-34
If you will send me the recipe I can try to rebild it for you.
Ababi
---------- Original Message ----------

>Help....I want to mix a glaze that calls for frit 3191 and I don't

Ron Roy on sat 10 nov 01


Who are you?

I may be able to sub in frit 3134 but I need the recipe - let me know what
other frits you can get.

RR

>Help....I want to mix a glaze that calls for frit 3191 and I don't have any.
>We no longer have a distributer here in Louisville and I was wondering if
>there was a comparable substitute. Thanks! Tonya
>
>_____________________________________________________________________

Ron Roy
RR# 4
15084 Little Lake Rd..
Brighton,
Ontario, Canada
KOK 1H0
Residence 613-475-9544
Studio 613-475-3715
Fax 613-475-3513