Group:
I have 50 lbs of 200 mesh Moose Creek high potash feldspar now. 5 lb samples
are available to the first 10 people who email me off list (you pay for the
shipping on the samples). Also, I am working on a new wood fire body based
on the 80 Helmer-20 Neph Sye format. Part of the body will be soft calcined
after mixing and ground to a fine fluxed grog to produce better forming
character and lower shrinkage while retaining the desirable fired colors.
Any testers out there who want samples? Same deal, shipping costs only.