Erik Buitenhuis on fri 16 nov 01
Hi all,
I would like to increase the temperature that my electrical oven can reach. From 'The art of firing' by N. Lou I understand that spraying it with ITC100HT would help. Now I have two problems: (1) The European retailers of ITC in Danmark haven't replied to my query, and (2) I don't really want to buy a gallon for my 40 L oven. So: Who will sell me 250 ml (about 1/20th of a gallon) of ITC100HT. I would appreciate it.
Best regards,
Erik Buitenhuis.
--
_______________________________________________
1 cent a minute calls anywhere in the U.S.!
http://www.getpennytalk.com/cgi-bin/adforward.cgi?p_key=RG9853KJ&url=http://www.getpennytalk.com
Russ Fish on fri 16 nov 01
Most pottery supply stores in the U.S. also carry pints of the ITC 100HT. I
buy mine by calling 901 947-9218. Or Fax Feriz Delkic of ITC to ask for his
distributors in Europe. The fax number is 904 273-1616.
Good Luck,
Russ
----- Original Message -----
From: "Erik Buitenhuis"
To:
Sent: Friday, November 16, 2001 6:51 AM
Subject: Who will sell me some ITC100HT?
> Hi all,
>
> I would like to increase the temperature that my electrical oven can
reach. From 'The art of firing' by N. Lou I understand that spraying it with
ITC100HT would help. Now I have two problems: (1) The European retailers of
ITC in Danmark haven't replied to my query, and (2) I don't really want to
buy a gallon for my 40 L oven. So: Who will sell me 250 ml (about 1/20th of
a gallon) of ITC100HT. I would appreciate it.
>
> Best regards,
> Erik Buitenhuis.
>
> --
>
> _______________________________________________
> 1 cent a minute calls anywhere in the U.S.!
>
>
http://www.getpennytalk.com/cgi-bin/adforward.cgi?p_key=RG9853KJ&url=http://
www.getpennytalk.com
>
>
>
>
____________________________________________________________________________
__
> Send postings to clayart@lsv.ceramics.org
>
> You may look at the archives for the list or change your subscription
> settings from http://www.ceramics.org/clayart/
>
> Moderator of the list is Mel Jacobson who may be reached at
melpots@pclink.com.
>
| |
|