Darlene Beverlin on tue 20 nov 01
Use HOT glue sticks. sorry I did not make that clear. But the hot glue =
sticks work great.
darlene
----- Original Message -----=20
From: Darlene Beverlin=20
To: clayart=20
Sent: Tuesday, November 20, 2001 12:09 AM
Subject: new (I think) way of making small molds
Once in a blue moon (that was last weekend) my friend Lucy comes over =
and we brainstorm for a bit.=20
She wanted to make sushi dip bowls to accompany my fish platters as =
gifts for her family.
So to make a few quick molds of a shell, I sprayed PAM on the exterior =
of the shell and started squirting glue. About 3 sticks of glue per med =
shell makes an adequate mold. 4 is better. The dried glue is flexible =
enough to release a curved shape easily. =20
I like them so well I am going to being to produce them. =20
I had a blast. Lucy got her Christmas gift making done. I got 3 new =
products to develop (Bill says I have to take off 6 if I add 3) And, =
Lucy owes me some production time later on. hhehehhe little does she =
know she might be making 200 sushi/butter dishes. =20
have fun all
darlene