search  current discussion  categories  techniques - misc 

peeling wax resist

updated mon 26 nov 01

 

jessica sletten on sun 25 nov 01


Greetings. I used Forbes wax over the glaze on
the rim of a bowl and when I returned the next
day, the wax was cracked and peeling. I keep my
studio around 52 degrees when I'm not working in
it. Does anyone know if the cool temperatures
caused the wax to peel, or if perhaps the glaze
was not dry enough when I applied the wax. I
thought the glaze was dry. Thanks for any help.

Jessie
New Richmond, Ohio