MOLINA, RAFAEL on tue 27 nov 01
a rchives
Jim Bob:
I sent in this recipe. It's in the archives listed item # 030685, date
98/02/22, subject - glaze formula reply.
Here is a copy of the original message:
Thought I would send this recipe Jeremy requested out to the whole
group. It's a very nice gloss black glaze. I acquired the recipe from
Dennis Olson who used this quite extensively with masking and
sandblasting which resulted in a nice high fire "black on black" surface.
Black ^ 10 reduction (from Dennis Olson)
Dolomite 300
Whiting 360
Soda Feldspar 4020
EPK Kaolin 300
Flint 1020
Cobalt Carbonate 180
Red Iron Oxide 240
Bentonite 60
Ciao,
Rafael
Rafael Molina, MFA
Assistant Professor of Art
Department of Music, Art, and Dance
Tarrant County College-Southeast Campus
2100 Southeast Parkway
Arlington, TX 76018-3144
(817) 515-3711
(817) 515-3189 fax
-----Original Message-----
From: Jim Bob Salazar [mailto:jsalazar@SULROSS.EDU]
Sent: Tuesday, November 27, 2001 11:13 AM
To: CLAYART@LSV.CERAMICS.ORG
Subject: black glaze, dennis olsn, archives
hey folks,
could some prompt me on how to do a successful search in the archives? i
was
recently sent a dennis olson black glaze recipe from someone on list and i
had a
crash and now can't find the glaze. went to the archives and it told me
there was
no match. can someone help me?
thanks in advance,
jim bob
____________________________________________________________________________
__
Send postings to clayart@lsv.ceramics.org
You may look at the archives for the list or change your subscription
settings from http://www.ceramics.org/clayart/
Moderator of the list is Mel Jacobson who may be reached at
melpots@pclink.com.
| |
|