search  current discussion  categories  kilns & firing - bricks 

cheap(er) ifb in la area?

updated wed 28 nov 01

 

Lajos Kamocsay on tue 27 nov 01


Hello,

Thanks for all the response to my 2.5" kiln wall question. To bring down =
cold face temperature and to improve efficiency I'll build my kiln with =
4.5" walls.
Now I need those IFBs... Laguna sells a 25 box of K26s for ~$108. Is =
there a more affordable source in the LA area?

Thanks,
Lajos

Jim Bob Salazar on tue 27 nov 01


hey there,

i've got a buddy who sells ifb. he is in texas but who knows, he might be able to get you a deal. get in touch with chris hart at landsquid@yahoo.com hope
this helps.

jim bob