search  current discussion  categories  materials - barium 

strontium matt error

updated fri 30 nov 01

 

Lesley Alexander on thu 29 nov 01


Oh boy! Thanks, Bob. The Neph Sy should be 60, not 20; I copied wrong.
So his recipe is:
Neph Sy 60
Lithium 1
Ball clay 10
Stront carb 20
Silica 9
Add 2% bentonite. And That's 100 + 2%. Lesley