The most recent information I have,(Interceram 5/2001) is that BHS =
Tabletop division are bisquing porcelain flatware to 1100 Celsius in 19h =
30m cold to cold, then glost firing to 1420 Celsius in 7h 00m cold to =
cold. Production rate is 55,000 units per week on a three shift basis, =
giving an annual production of 20,000,000 units. All automated =
production.