silica glass (sio2) data sheet

updated mon 24 dec 01

 

GlassyClass on fri 21 dec 01


says that silica glass has a soften point of 1600C

http://www.crystran.co.uk/sio2data.htm


begin 666 Silica Glass (SiO2) Data Sheet.url
M6T1%1D%53%1=#0I"05-%55),/6AT=' Z+R]W=WM3,#@S,C(S,T(X.$%#,3 Q-4,-"@``
`
end

Bruce and Lynne Girrell on sun 23 dec 01


GlassyClass wrote:

> Silica Glass (SiO2) Data Sheet
> says that silica glass has a soften point of 1600C
>
> http://www.crystran.co.uk/sio2data.htm


which is substantially higher than cone 10 (about 1285ºC). Sounds like it
ought to work as a window. Fused silica also has close to zero expansion.

Bruce "too hot baby" Girrell