Lee Marshall on fri 4 jan 02
help. i am at my wits end with my electric kiln. it's an L & L J230
manual.i've changed switches,elements etc. and have exhausted my expertise.
before i break down and send the whole controller assy to l&l does any one
out there know of a kiln doctor in the nashville ares that makes house calls.
i've tried an electrician that has worked with kilns but that has not worked
well because she doesn't carry the parts.
thanks in advance for you help
lee
lee marshall
lmarsh1220@aol.com
615-286-1264
william schran on sat 5 jan 02
Lee - I have 2 J230's (also have J18's & a J2927) at school that I've
completely rebuilt the electrical components over the years. What's
the problem you're having?
Bill
| |
|