search  current discussion  categories  glazes - traditional iron glazes 

my versions to falls creek shino

updated tue 29 jan 02

 

Ababi on mon 28 jan 02


Just now, I visited my web site. in the second glaze tests page
their are slides: "falls 6" my version to Falls Creek Shino
"falls11" my version to Falls Creek Shino with
Zinc oxide
Try http://members4.clubphoto.com/ababi306910/516875/
If not, through the regular way.
http://members4.clubphoto.com/ababi306910/
Ababi Sharon
Kibbutz Shoval- Israel