search  current discussion  categories  materials - misc 

china clay and kaolin question

updated thu 31 jan 02

 

Marianne Lombardo on wed 30 jan 02


I was looking at a glaze recipe in the archives that calls for both =
China Clay and Kaolin. I'm wondering what the difference is. I thought =
Kaolin was a China Clay? =20

Marianne Lombardo
Omemee, Ontario, Canada