Just put totally dry clay, little pieces,trimmings or something in a cup =
or lidded container and cover the trimmings with water. It just really =
doesn't matter how much. I want mine to be thick because I like the =
spooze to be pasty but you can use it more like a liquid also. If you =
get it too watery just leave the container open for a few days and it =
will thicken up.
Good luck, Susan Parrish