Alisa og Claus Clausen on mon 11 feb 02


Dear Clayart,
Some of you have written that some of your results are very different for
mine, including the Saffire blue, Gibby's wild rose Tenmoku and the Xavier
green. I have tested Xavier several times and always get a green
gloss. Further, the wild rose Tenmoku is sometimes more glittery, but more
or less in the same range of semi glossness and brown/blackness. This is
the first time that I tried the Saffire blue. When I get back, for
interest sake, I will retest the Saffire blue. Test results will be
different of course and that is why we test them. The majority of my basic
raw materials are also sourced differently than those working in the
USA. So, that was this group of tests. I do not have a site or way to
post these results as of now.
regards from Alisa it is 6.32 am and I signing off Clayart for now and
making my toast.

Mert & Holly Kilpatrick on mon 11 feb 02


We always get a definitely glossy glaze from Xavier green also, and that is
with a slow cooling down.

Holly

From: "Alisa og Claus Clausen"

> Dear Clayart,
> Some of you have written that some of your results are very different for
> mine, including the Saffire blue, Gibby's wild rose Tenmoku and the Xavier
> green. I have tested Xavier several times and always get a green
> gloss.

becky schroeder on mon 11 feb 02


hmmmmm, i always get a lovely satin matte finish.

becky schroeder


>We always get a definitely glossy glaze from Xavier green also, and that is
>with a slow cooling down.
>
>Holly
>
>From: "Alisa og Claus Clausen"
>
> > Dear Clayart,
> > Some of you have written that some of your results are very different
>for
> > mine, including the Saffire blue, Gibby's wild rose Tenmoku and the
>Xavier
> > green. I have tested Xavier several times and always get a green
> > gloss.
>
>______________________________________________________________________________
>Send postings to clayart@lsv.ceramics.org
>
>You may look at the archives for the list or change your subscription
>settings from http://www.ceramics.org/clayart/
>
>Moderator of the list is Mel Jacobson who may be reached at
>melpots@pclink.com.


_________________________________________________________________
Join the world’s largest e-mail service with MSN Hotmail.
http://www.hotmail.com