Jon Pacini on thu 14 feb 02


Greetings All----A bunch of you have been awaiting this info on Arroyo slip.
For the uninitiated Arroyo Slip is a mineral similar to Albany or Alberta
Slip.



SiO2 4.877 MOL 64 %
Al2O3 .643 14.3
Fe2O3 .243 8.5
TiO2 .053 .9
MgO2 .397 3.5
CaO2 .314 3.8
K2O3 .170 3.5
Na2O3 .120 1.6

mol. wt. 458.56
COE 3.98x10 -6
LOI 8.05

Jon Pacini
Clay Manager
Laguna Clay Co