clear glaze and slow cooling

updated sat 16 feb 02

 

Marianne Lombardo on fri 15 feb 02


I've only used this twice, but both times were in a slow cooling. It =
was a very clear, nice glaze on white stoneware. On red clay however, =
little wisps of blue (not unattractive) were in the clear.

William Edwards 1.2.3.4 Clear Gloss ^6
EPK 30.0
Flint 20.0
Frit 3134 40.0
Wollastonite 10.0

Marianne Lombardo
Omemee, Ontario, Canada