search  current discussion  categories  kilns & firing - shelves & furniture 

shelves for salt glazing.

updated sat 23 feb 02

 

Mitsuru Cope on fri 22 feb 02


An addition to Ivor Lewis, there is an explanation of Sandra Johnstone's
method of stacking in Salt-Glaze Ceramics by Janet Mansfield pages 16-17.
Mitsuru

> An apology relating to my post about this. I should have checked my
> references. It is Sandra Johnstone. My mistake in writing Johnson.
> Sorry about that Folks.
> Full reference is:
> Sandra Johnstone, "Salt Firing Without Kiln Shelves". Ceramics '88. 5th
> National Ceramic Conference. Proceedings, May 1988. Sydney, Australia.
> Best regards,
> Ivor Lewis
>
> ______________________________________________________________________________
> Send postings to clayart@lsv.ceramics.org
>
> You may look at the archives for the list or change your subscription
> settings from http://www.ceramics.org/clayart/
>
> Moderator of the list is Mel Jacobson who may be reached at
> melpots@pclink.com.
>