Llewellyn Kouba on fri 1 mar 02
I fired the gas kiln this past Monday and had 75 wonderful works. Not a
thing failed. I will try and get back to you on how the test tiles went. I
had mixed all of Tom Coleman's pigment group but at cone 9 they mostly
burned out which is what I was expecting. No doubt though they would be
wonderful at cone 8 or below? Photos and web page will be upgraded as time
permits.
Llewellyn
| |
|