Cindy Strnad on sun 3 mar 02


See Ron and John's book, "Mastering Cone 6 Glazes" for the recipe.

This is a pretty glaze, glossier than the others. More green than blue and a
little more opaque than I like, but I generally prefer transparent glazes. I may
try this with less Rutile and/or less copper or more cobalt. Then I will call it
Caribbean Sea Blue-Green. Or Turquoise, maybe.

(see notes in separate post on firing specifics)
=====================================
Cindy Strnad
Earthen Vessels Pottery
RR 1, Box 51
Custer, SD 57730
USA
cindy@earthen-vessels-pottery.com
http://www.earthen-vessels-pottery.com
CM Critique discussion forum
http://www.earthen-vessels-pottery.com/toforum.html