mel jacobson on mon 4 mar 02
you have more than enough.
i suggest:
use a blender and blend that stuff for about 5 minutes
with a water. you want it thin. and very well mixed.
it comes with junks...we hate them.
when you are finished let them hang (coils) to dry over night.
you will find it hard to know if you got the 213 on the
coils...just run them through the mud pan a couple of times.
when you are done, you will have a pint and a half of
213 left. put the cover on tight.
(how do you get one and a half pints in a one pint
jar? you figure that one out.
mel
From:
Minnetonka, Minnesota, U.S.A.
web site: http://www.pclink.com/melpots
| |
|