search  current discussion  categories  glazes - specific colors 

variegated slate blue

updated tue 5 mar 02

 

Cindy Strnad on sun 3 mar 02


For recipe, see "Mastering Cone 6 Glazes" by Ron & John

In character, this seems much like the photo in the book, but in hue, I got it
much more green. I suspect my (lavender) cobalt carb is not as strong as theirs.
It is a nice color, but I'm going to add another portion of cobalt and try
again.

(see notes in separate post on firing specifics)
=====================================