search  current discussion  categories  glazes - misc 

mastering glazes - modific

updated sat 9 mar 02

 

Mediaone on thu 7 mar 02


Dear John or Ron,

The Glossy Base Glaze 1 (p.92, Mastering Cone 6 Glazes) requires G200. =
But I am out of it, and thinking about substituting G200 with Custer =
Feldspar. If I change to:
Custer spar =3D20
Frit 3134 =3D20
Wollastonite =3D 10.5
EPK =3D 20
Talc =3D 11.5
Silica =3D 18

The Unitiy molecular formula is practically the same. Is there any =
problem with my substitution? Your comment would be appreciated. =
Mariko

John Hesselberth on fri 8 mar 02


on 3/7/02 10:08 PM, Mediaone at marikocruse@MEDIAONE.NET wrote:

> The Unitiy molecular formula is practically the same. Is there any problem
> with my substitution? Your comment would be appreciated. Mariko

Hi Mariko,

Custer and G-200 are pretty similar so there shouldn't be any problem, but
try it and see. Test, test, test.

John

Web sites: http://www.masteringglazes.com and http://www.frogpondpottery.com
Email: john@frogpondpottery.com