I've added a page on color response of some common colorants to my base
cone 9-10 crystalline glaze.
You can visit it at http://home.earthlink.net/~bsondahl/cryscolor.html
Brad Spndahl
--
For original art, music, pottery, and literature, visit my homepage
http://home.earthlink.net/~bsondahl/
Pottery salespage http://sondahl.freeyellow.com
New music site at mp3.com http://www.mp3.com/sondahl
william schran on sun 24 mar 02
Brad - Thanks for taking the time & energy to go through the color
tests. Were these tests done on stoneware or porcelain? I'm asking
because the backgrounds are a grayish color and I didn't know if that
was the color from the photo images or actual color.
Are you using feldspar & kaolin in your glazes simply to retard glaze
flow to avoid using extra catch basins?
Thanks, Bill
| |
|