Debbie Jestin on sun 24 mar 02
I'm moving to Vancouver Island to an acreage and there's no gas, so I have a
basically new Torch Bearer 2327G for sale. It's got 3 burners, 80,000 BTU,
cone 10, Dawson Automatic shut-off, igintion ring, magnetic shut off valve,
kiln vent, shelves, etc. Fired 5 times. 2500.00 cdn. If interested email me.
No more winters for me
cyberscape on mon 25 mar 02
Debbie,
You can switch the orifices and fire that kiln with propane. Olympic
will send you the correct orfices. Call em.
Harvey Sadow
| |
|