search  current discussion  categories  materials - rutile 

rutile rutile rutile

updated wed 27 mar 02

 

Earl Brunner on mon 25 mar 02


Albany moderates cobalt nicely, for brushwork.

Earl Brunner
mailto:bruec@anv.net
http://coyote.accessnv.com/bruec


-----Original Message-----
From: Ceramic Arts Discussion List [mailto:CLAYART@LSV.CERAMICS.ORG] On
Behalf Of Ann Brink
Sent: Monday, March 25, 2002 1:00 PM
To: CLAYART@LSV.CERAMICS.ORG
Subject: Rutile rutile rutile


PS- I also got about 10 lbs of Albany slip. I know it will make a
brownish
shiny glaze, but does anyone have another favorite use for it, perhaps
as a
wash combined with something?



________________________________________________________________________
______
Send postings to clayart@lsv.ceramics.org

You may look at the archives for the list or change your subscription
settings from http://www.ceramics.org/clayart/

Moderator of the list is Mel Jacobson who may be reached at
melpots@pclink.com.

Ann Brink on mon 25 mar 02


I for one am not bored reading about rutile. I recently used up the last of
my light rutile, and now have dark rutile (I bought a lot of misc. materials
from another potter). There will be tests in my next firing, but I don't
know if I should be anxious or eager.

Ann Brink in CA

PS- I also got about 10 lbs of Albany slip. I know it will make a brownish
shiny glaze, but does anyone have another favorite use for it, perhaps as a
wash combined with something?