Lajos Kamocsay on thu 28 mar 02
hello,
i've tried the holly red glaze from laguna, ^06. the color and shine is =
amazing! it also gives great texture with rutile. no pinholing, no =
crazing.
however, it contains lead. can i get the same deep red using some =
different flux? any recepies?
thanks,
Lajos
Ababi on thu 28 mar 02
The red in this case comes from the lead!
---------- Original Message ----------
>hello,
>i've tried the holly red glaze from laguna, ^06. the color and shine is
>amazing! it also gives great texture with rutile. no pinholing, no
>crazing.
>however, it contains lead. can i get the same deep red using some
>different flux? any recepies?
>thanks,
>Lajos
>________________________________________________________________________
>______
>Send postings to clayart@lsv.ceramics.org
>You may look at the archives for the list or change your subscription
>settings from http://www.ceramics.org/clayart/
>Moderator of the list is Mel Jacobson who may be reached at
>melpots@pclink.com.
| |
|