Craig Martell on thu 28 mar 02


Hello Alex:

Thanks! The teapot and cups have five or six different slip colors applied
by spraying, brushing, trailing, and applied dots of fusible
colorant. After the bisque, I line them and dip the tops and bottoms in
the tenmoku and then spray on the ash glaze. Then I take a
vacation! :>) No wait, I have to fire all that stuff first.

I wouldn't worry too much about a long line to buy my teapots.

nice to hear from you, Craig Martell in Oregon

John Weber on sat 30 mar 02


Craig, what do you mean by "dots of fusible colorant"?

-----Original Message-----
From: Ceramic Arts Discussion List [mailto:CLAYART@LSV.CERAMICS.ORG]On
Behalf Of Craig Martell
Sent: Friday, March 29, 2002 12:30 AM
To: CLAYART@LSV.CERAMICS.ORG
Subject: Re: really nice teapot/Alex


Hello Alex:

Thanks! The teapot and cups have five or six different slip colors applied
by spraying, brushing, trailing, and applied dots of fusible
colorant. After the bisque, I line them and dip the tops and bottoms in
the tenmoku and then spray on the ash glaze. Then I take a
vacation! :>) No wait, I have to fire all that stuff first.

I wouldn't worry too much about a long line to buy my teapots.

nice to hear from you, Craig Martell in Oregon

____________________________________________________________________________
__
Send postings to clayart@lsv.ceramics.org

You may look at the archives for the list or change your subscription
settings from http://www.ceramics.org/clayart/

Moderator of the list is Mel Jacobson who may be reached at
melpots@pclink.com.