search  current discussion  categories  glazes - misc 

glaze ballclay patch

updated thu 4 apr 02

 

James Clark on wed 3 apr 02


Hi all,
We just had a lid com out of a cone 6 glaze firing with a slight s- crack
in it. I read
somewhere about mixing ball clay with the glaze, filling the hole and
refiring the piece. Has anyone heard of this and if so what consistency
should the mixture be and how do you apply it?
Thanks in advance