Jeff Seefeldt on sun 7 apr 02


I've been having problems with my wall mount controller, found out it was
something I was doing rather than a faulty controller.

Just wanted to tell everyone of good experiences with Neal at Skutt,, he
made several phone calls to my house,,, walked me through several
suggestions,, I test fired it over the weekend with shelves and only a few
pieces. Perfect ^6 at the thermocouple on both ramp mode and cone mode.


Jeff