Chris and Nissa on tue 9 apr 02


Thanks RR and Margaret your advice was very helpful and the glaze turned out
beutiful for the appearance of brown hair on a bear sculpture. Thank you
again.

Chris Koivisto
Duluth

-----Original Message-----
From: Ceramic Arts Discussion List [mailto:CLAYART@LSV.CERAMICS.ORG]On
Behalf Of Ron Roy
Sent: Monday, April 01, 2002 12:10 AM
To: CLAYART@LSV.CERAMICS.ORG
Subject: Re: Fwd: Re: Leather ^6 GB Sub?/Thanks


Hi Chris,

I'm late with this - been on the road and still trying to catch up.

Margaret asked me to comment on her frit 3134 revision - looks good to me.

You may find it needing some more work - make sure you give as much detail
to Margaret as possible - including cone bend.

Most glazes - when revised this way will work just fine in most cases. The
unbalanced ones - like this one - are the most difficult.

Margaret is also right about the durability - this glaze is going to change
in use - and it could be dramatic - try a slice of lemon overnight on it.

Margaret is getting very good at this folks - takes some of the weight off
me and I am grateful for that.

RR


____________________________________________________________________________
__
Send postings to clayart@lsv.ceramics.org

You may look at the archives for the list or change your subscription
settings from http://www.ceramics.org/clayart/

Moderator of the list is Mel Jacobson who may be reached at
melpots@pclink.com.