Dear Jocelyn McAuley,

You will have to sinter your PMC first, then mould or form your ceramic =
clay about the metal.

Next comes the hard part. You have to refire at a temperature lower than =
the MP of the PMC.

>From what I have read over the past three or four years this stuff is =
very tight when it comes to firing temperatures, only a few degrees =
difference between getting good sintering and melting to destruction.

Never tried the stuff, much to expensive to import. With Bullion Silver =
less than $US 5:00 per ounce troy a few shares in the manufacturer would =
seem to be a good speculative investment.

Best regards,

Ivor