Imzadi . on mon 15 apr 02
In a message dated 4/15/02 5:14:11 AM Pacific Daylight Time,
dupremm@MSTP.QUANTICO.USMC.MIL writes:
<< Had a wonderful deep red and a
surprise bonus of a deep black on some tiles I'm testing. The red were
achieved with Ron and John's Raspberry glaze, tweaked with just a touch
more
nickle. The black I got with Hendley's Substitute for Albany slip and 5%
cobalt oxide. Just a shade too matt for my tastes, but who knows?
>>
| |
|