The use of squares of drywall to dry tiles came up recently (using
sandwiches of green tiles between drywall chunks).

How do you keep pieces of gypsum, which have a way of flaking off cut
drywall, from getting into your clay and doing the old plaster-in-clay
damage? I'm not asking about the tiles themselves, but about general
studio housekeeping tips when using drywall.